显示标签为“Taphole Brick”的博文。显示所有博文
显示标签为“Taphole Brick”的博文。显示所有博文

2013年10月22日星期二

Taphole Brick



Introduction:
Taphole Brick is molded at isostatic pressure, with fused magnesia and graphite as raw material. It is characterized by good oxidation resistance, high strength, good corrosion resistance, good integrity, easy replacing and long life and it is ideal material taphole of large and medium furnace.
Specific Application: Eccentric bottom tapping.
Service Life: Smelt steel scrap, 60 heats MIN; smelt molten iron and scrap steel, 200 heats MIN.
Payment Terms: L/C, T/T

For physical and chemical indexes, click here.
For more products, click here.

Taphole Brick



Introduction:
Taphole Brick is molded at isostatic pressure, with fused magnesia and graphite as raw material. It is characterized by good oxidation resistance, high strength, good corrosion resistance, good integrity, easy replacing and long life and it is ideal material taphole of large and medium furnace.
Specific Application: Eccentric bottom tapping.
Service Life: Smelt steel scrap, 60 heats MIN; smelt molten iron and scrap steel, 200 heats MIN.
Payment Terms: L/C, T/T

For physical and chemical indexes, click here.
For more products, click here.

2013年8月28日星期三

Taphole Brick


Refractory Brick>Taphole Brick

Introduction

Taphole brick is molded at isostatic pressure, with fused magnesia and graphite as raw material. It is characterized by good oxidation resistance, high strength, good corrosion resistance, good integrity, easy replacing and long life and it is ideal material taphole of large and medium furnace.

For physical and chemical indexes, click here.
For more products, click here.

2013年7月26日星期五

Taphole Brick



Introduction:
Taphole Brick is molded at isostatic pressure, with fused magnesia and graphite as raw material. It is characterized by good oxidation resistance, high strength, good corrosion resistance, good integrity, easy replacing and long life and it is ideal material taphole of large and medium furnace.
Specific Application: Eccentric bottom tapping.
Service Life: Smelt steel scrap, 60 heats MIN; smelt molten iron and scrap steel, 200 heats MIN.
Payment Terms: L/C, T/T

For physical and chemical indexes, click here.
For more products, click here.
Enhanced by Zemanta