What are the refractory materials used in induction furnace

Induction furnace is more commonly used in a melting metal furnace, the current mainly used to melt molten iron, molten steel, copper, aluminum, according to the different melting products, the use of different Medium frequency induction furnace refractory lining materials.
General melting molten iron, the use of quartz sand dry vibration refractory material;
Melting molten steel, using magnesia or alumina material;
Aluminum is made of alumina or clay.
Specific to the furnace, also divided into: coil mud, mouth, mica and insulation layer, dry vibration material layer. General mouth with plastic.

More refractory material:
What are the refractory materials used in induction furnace

E-mail:sales8@chinaelong.com

2017年7月28日星期五

Continuous smelting and repair of induction furnace

refractory material for induction furnace
refractory material for induction furnace
1.Continuous furnace
To reduce the repeated heat that caused by quenching furnace lining cracking, continuous smelting is very induction furnace refractory lining materials important for the extension of lining service life, it has caused attention of many users. If can not continuous use, intermediate frequency furnace in after a single use, want to join metals in furnace burden, and cover induction furnace lining material the furnace cover, it can not only give metal furnace material preheating, also can prevent the lining cracks caused by rapid cooling.

2.The Repair
(1) The intermediate frequency furnace Refractory company reach to 20 heats then need to tear down all of my throat opening, purpose is to check whether the furnace lining is drill iron, also check the dry lining loosening clearance. To repair the oven, it is best to use high metal front ring, and pay special attention to the old and new interface cleaned up. During the refractory brick next furnace operation, it should open first time below the fettling interface.
(2) The furnace mouth and throat opening is often slagging, impact erosion and burden, it need constant maintenance and repair, to ensure the normal dimensions of intermediate frequency furnace.

Article source:
Continuous smelting and repair of induction furnace

E-mail:sales8@chinaelong.com

Refractory Material, Fire Bricks, Refractory Manufacturer, China Refractory - CX Refractories

Refractory Material, Fire Bricks, Refractory Manufacturer, China Refractory - CX Refractories