Application of Ladle Castables
Because the water content of the whole
ladle castable is large, and the material structure is dense, the water is not easy to be discharged. Therefore, in the ladle baking process, the small heat is long, gradually warming up, preventing rapid heating, and the principle of roasting the fire is strictly prohibited, otherwise the ladle appears. It collapsed and peeled off. Bake with a baking machine and bake in a 72-hour system. The specific distribution is as follows:
Firstly, small fire stage: no less than 3 shifts, 24 hours (only 1/2 gas, no cover);
Secondly, medium fire stage: no less than 3 shifts, 24 hours (only 1/3 gas is added, plus a little wind, stamped);
At last, fire stage: no less than 3 shifts, 24 hours (open gas, add foot, cover)
Article source:
http://www.yilongrefractory.com/news/Application%20of%20ladle%20castables.html
E-mail:sales8@chinaelong.com
Application of Ladle Castables
回复删除Because water content of the whole ladle castable is large, and material structure is dense, the water is not easy to be discharged. Therefore, in the ladle baking process, the small heat is long, gradually warming up, preventing rapid heating, and the principle of roasting the fire is strictly prohibited, otherwise the ladle appears. ......
Article source:
http://www.yilongrefractory.com/news/Application%20of%20ladle%20castables.html
E-mail:sales8@chinaelong.com